Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube

Y & G International Trading Company Limited
Contact Now

Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube

Brand Name : Y & G

MOQ : Negotiation

Payment Terms : L/C, T/T

Supply Ability : 8000MT/Month

Delivery Time : 25-35 days

Packaging Details : Exporting package/wooden box / per customers’ requirement

Price : Negotiable

Material : UNS S32750,S31803, S32205, S32760

Standard : SA789,A790

Type : Seamless,Welded

OD : 1/4inch~24inch

Wall Thickness : SCH10S , SCH10, SCH20, SCH30, SCH40S...

Application : Heat exchangers and coolers

Surface Treatment : Varnish, Oil-dip, Passivation, Phosphating, Shot Blasting

Delivery Status : Annealed, normalized, normalized+Tempered, etc

Contact Now

SA789 UNS S32750 Stainless Steel Tubing Super Duplex Stainless Steel Pipe / Tube 25.4 * 2.11mm

Product Standard: ASME SA789
Main steel grades:
UNS S32750,S31803, S32205, S32760

Application: For heat exchangers and coolers and devices that are resistant to seawater, such as high temperature and concentrated nitric acid, such as oil refining, fertilizer, papermaking, petroleum, and Foundry

Features:

1.Superior resistance to general and local corrosion, especially to stress corrosion, pitting corrosion, crevice corrosion, corrosion fatigue and abrasion & corrosion.

2.Good weldability

3.Good mechanical properties

4.Excellent intergranular corrosion resistance

5.High cost-effectiveness, long life time

Chemical Composition & Physical Properties:

Grade

C

max

Si

max

Mn

max

P

max

S

max

Cr Ni Mo N
UNS S32750 0.030 0.8 1.2 0.030 0.015 24.0-26.0 6.0-8.0 3.0-5.0 0.24-0.32
UNS S31803 0.030 1.0 2.0 0.020 0.020 21.0-23.0 4.5-6.5 2.5-3.5 0.08-0.20
UNS S31500 0.030 1.0 1.2-2.0 0.030 0.030 18.0-19.0 4.5-5.5 2.5-3.5 0.05-0.10

Grade Y.S.MPa min T.S.Mpa min Elongation % Hardness HRC
UNS S32750 550 800 15 20
UNS S31803 450 620 25 20
UNS S31500 440 630 30 20

Mark: As required.

Inspection and Test: chemical composition test, mechanical properties test(tensile, yield, elongation), process properties test(flatting, flaring, bending, hardness, impact, etc.), appearance and size test, non-destructive inspection test, hydrostastic test.

Delivery status: Annealed, normalized, normalized+Tempered, etc.

Surface treatment: oil impregnation, paint, passivation, phosphating, shot blasting etc.

Packing: Exporting package/wooden box /as requirement.

Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube


Product Tags:

stainless steel pipe

      

polished stainless steel tubing

      
Wholesale Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube from china suppliers

Pitting Corrosion Resistant Stainless Steel Round Tube , High Precision S32750 Stainless Tube Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Y & G International Trading Company Limited
*Subject:
*Message:
Characters Remaining: (0/3000)